Durometro per prove Shore e IRHD

 

 

Tests on rubber, thermoplastic and vulcanized rubber samples with IRHD method

 

Fully automatic test cycle

 

Load cell with electronic Closed Loop control system

 

 


 

 

Few easy steps to perform the hardness test!
 

 

 

 
 

Position the sample to be tested on the anvil

 

Move the anvil close to the indenter using the handwheel

 

Press the “START” button

 

 

 

 


 

 

Shore e IRHD hardness tester

 

 


 

 The MicroIRHD DX-13 has a computer with a pre-installed software to fully manage the machine and to analyse data. The interface is very intuitive and it is managed through the 10.4’’ touchscreen. Using the USB and Ethernet ports, it is possible to connect the instrument with network cards, printers, etc.

 


 

 

 Test methods

 

   DX - 13 A   DX -13 B   
 

N method:
For samples with thickness equal to or higher than 4 mm. Mostly used for rubbers with hardness between 35 IRHD and 85 IRHD, but it can also be used for samples between 30 IRHD and 95 IRHD

 

M method:
For samples with thickness equal to or lower than 4 mm. Mostly used for rubbers with hardness between 35 IRHD and 85 IRHD, but it can also be used for samples between 30 IRHD and 95 IRHD

 
   

H method:
For samples with thickness equal to or higher than 4 mm and hardness between 85 IRHD and 100 IRHD

     
   

L method:
For samples with thickness equal to or higher than 6 mm and hardness between 10 IRHD and 35 IRHD

     

 

 

 Technical data

 

Operatin mode Automatic - PC interface 
Start up Cell and Closed Loop (patented)
Working depth 73 mm  
Connectiones RS 232 Standard, PC: 2x USB, 2x Ethernet, PS/
Power supply 220 Vac 50÷60 150VA
Field of use Plastic materials (rubber, thermoplastic) 
Standards ISO 48, 7318, 7619, ASTM 1415, ASTM 2240